![Transcription Center logo](/themes/custom/tc_theme/assets/image/logo.png)
This transcription has been completed. Contact us with corrections.
•252°-->300° pitting noted on tang surface (<.005") [no burnishing previously on this segment - would probably be in paperwork .... might have had some work done @ MTI] (this is fairly common)[use shim stock] •R aft center segment left outside bec. of req. of only 1 seg inside at once. Rained. Cleaned out H2O, dried off insulation. •2 O-ring bags were rejected at KSC •talk to technician who observed mating operation. MOSER, LEE, LITTLES smoke ~.5 sec --> ~4 sec some photos may indicate smoke lasts until ~12 sec (not verified) plume: 45° ± 10°(~315° ± 10°) joint ± 1 ft