Viewing page 184 of 309

This transcription has been completed. Contact us with corrections.

to mix w/ cement already 5x used & good result
same heat of firing
tobong uses less fuel
[[strikethrough]] formerly 20,000 wood a firing,
now 10,000
sampah 15,000 sepeda x
1000 Rp@ [[/strikethrough]]

[[4 column table]]
|[[blank]]|kayo bakar|sampah|jerami (damen)|
|dulu|5000 (potongan from coconut sawmill) (1500 a sepeda)|15 sepeda @1000=15,000|10 pepeda @750(buy)=7500|
|now|5000 (same)| 2 sepeda @1000|1 jerami cari|
[[/4 column table]]

so befor 27,500 a firing, now 7000