[[underlined]] Amneoplastics [[/underlined]]
H2SO4 [[overwritten]] (85%) [[/overwritten]] (25%) after 7 days beginning attach, but no action whatever after 25 hours, at 16°C
NaOH 10% = after 7 days no attach beginning
attach ^[[after]] 2-3 weeks
HCl (10% HCl) one day no attach 
No action by soap nor Na2CO3 nor oils.
Cyandiamid obtainable 1 mark per kilo in Jugoslavia from electrochemical works- (I believe process is patented)
Chromeplated molds - ^[[Lam?]] or new alloy
Laminated.
True white unsized paper used; see printed sheets.
Aminoplastics dissolved in formaldehyde solution - [[strikethrough]] Fine cotton flo [[/strikethrough]] This solution sheets coated in its carrier by aluminum broad chain about 1 meter while acting
[[end page]]
[[start page]]
as an apron, travelling thru a flat aluminim tunnel, where heated and dried, then automatically rolled up then in hot hydraulic press, between aluminum or alloy glossy metal sheets. See sheet with printed matter
As for molding powder. Not yet succeeded preforming some powder obtained as follows:
Dissolve aminoplast in formaldehyde [[strikethrough]] Then this [[/strikethrough]] in aluminum kettles
This colorless solution impregnates fine cotton flock, then cotton flock is dried, then ground fine and ready for use.
Smell of CH2O indicates losses. See sheet of physical contants[[guess]] Sober inexpensive laboratory as compare to ours.